I've pretty much have a solid grip on using a humidity storm to address creases, dents and dings in Pokémon cards. The issue is typically once you're done the card will have an orange peel texture to it. There are a few ways to deal with that, and I'm experimenting with a hybrid approach.

This is a Blastoise holo I've been working on. I accidentally imprintrd a ripple texture into the back when I did a steam treatment with a protective parchment paper backer and left it in the heat press too long. I'm using a hybrid of the "Anaconda Squeeze" approach to fix it.
I've taken an acrylic card display slab and repurposed it for my process here. I bought some overside 4x6 penny sleeves and cut the sides open except for the bottom. Then, what I've done is applied 1-2 sprays of Kurt's card care spray and left the card in a card mat sandwich for an hour to humidify it.
After that, I cut the sides off of a brand new top loader. I sandwiched the card between the vinyl panels. That then goes into the oversized penny sleeve. The sleeve goes into the acrylic card holder. I line it up, screw it in place to keep things from moving, then apply the clamps at maximim pressure. Then, I tighten the screws down and leave it that way for a week.
I tried without the vinyl sheets and it worked on one side. The downside is it did leave some indents where the penny sleeve wrinkled. The vinyl won't wrinkle and will prevent dents, while the penny sleeve acts as a channel so moisture can still evaporate. That's my theory anyway. We'll see if I'm right when I remove the clamps next weekend. Hopefully it works!


Buy ELIXIR and stake to receive HIVE dividends!
Delegate to @nectarbytes to earn ELIXIR!https://tribaldex.com/trade/ELIXIRhttps://hive-engine.com/trade/ELIXIR

Buy DUO and stake to receive HIVE dividends, tip others, have your posts curated, and grow Hive!https://tribaldex.com/trade/DUOhttps://hive-engine.com/trade/DUO

Do you like stacking gold and silver?